My experience is that liquid chalk is a poor choice for wood. Over time the resin reduces the friction significantly. I would suggest a chalk ball if you don't want loose chalk flying around. If this isn't enough to keep sweat at bay then you'll be better placed doing some skin conditioning with Antihydral.